Briquetting of Ulexite Fines
By G. Ozbayoglu, Z. Ozdemir
Turkey is the main boron minerals producing country in the world. The most important boron minerals are tincal, colemanite and ulexite. All mining, beneficiation and handling operations generate fines
Jan 1, 2004
-
Regional geological and tectonic setting of porphyry deposits in Washington State
By R. Lasmanis
"Washington State's diverse geological setting is reflected by its several types of porphyry Cu-Mo deposits. All are associated with calc-alkaline intrusions, and they range in age from Jurassic
Jan 1, 1995
-
Concentration and Cyanidatton at Flin Flon Pilot Mill
By S. P. Lowe
Flotation testing of Flin Flon ore was started in the Denver laboratory of Complex Ores Recoveries Co. in March, 1926. There had been a considerable amount of flotation testing previously which had sh
Jan 1, 1930
-
Une Corrélation Génétique entre les Roches Granitiques, et les Dépôts Éluvionnaires, Colluvionnaires et Alluvionnaires de Columbo-Tantalite d'Issia, Centre-Ouest de la Côte d'Ivoire
By Robert Yobou, Jacques Naho, Benjamin A. Allou, Jacques Carignan, Huan-Zhang Lu, Jayanta Guha, Koffi Pothin
"Résumé - Les seules productions de columbo-tantalite en Côte d'Ivoire sont effectuées dans les éluvions, colluvions et alluvions d'Issia, au Centre-Ouest de la Côte d'Ivoire. Même si u
Jan 1, 2005
-
La Rentabilité
1 INFORMATIONS GÉOLOGIQUES ET PLANIFICATION MINIÈRE La notion de gisement exploitable s'appuie sur les connaissances de géologie, d'ingénierie et tablir la rentabilité en fonction des inves
May 1, 2002
-
A Review on the Initiation of Environmentally Assisted Cracking in Line Pipe Steel
By M. T. Shehata, R. W. Revie, M. Elboujdaini
Environmentally assisted cracks in linepipe steels are initiated either as a result of stresses in combination with environmental effects, as in stress corrosion cracking (SCC), or as a result of trap
Jan 1, 2005
-
Ventilation as a Means to Prevent Silicosis in Ontario Mines
By Clifford S. Gibson
THESE troubled times suggest three reasons for maximum effort to control silicosis: (1) To keep to a minimum the ever-increasing burden occasioned by past deficiencies in this respect. (2) To effe
Jan 1, 1942
-
Pyrolysis of Chrysotile Asbestos Fibre
By H. M. Woodrooffe
IT IS WELL KNOWN that chrysotile asbestos from various occurrences exhibits varied physical properties and certain differences in chemical corn position, both of which conditions may have an important
Jan 1, 1956
-
Influence of microstructural parameters of a SOFC composite cathode on the collection of reliable experimental data: A modelling analysis
By B. Kenney
For SOFCs, composite cathodes comprising an electronically conducting electro¬catalyst (e.g. LSM) and an conically conducting electrolyte material (e.g. YSZ) are considered to improve the electrochemi
Jan 1, 2005
-
The Behavior of Carbonaceous Matter in Gold Extraction
By H. Tan
The effect of carbonaceous matter on gold extraction was investigated in cyanide systems with pure gold as well as pre-robbing sulfide gold ores. Auger studies demonstrated that the carbonaceous matte
Jan 1, 2005
-
Wemco Large-Capacity Flotation Cells
By J. Graham Eby
"This paper describes the development and some typical applications of Wemco's large-capacity flotation machines, the No. 120 and the No. 144, with volumes of 300 and 500 cubic feet, respectively. Dur
Jan 1, 1972
-
Recovery of Iron from Waste Slag of Pyrite Processing Using Reduction-Roasting Magnetic Separation Method
By A. McLean, Q. R. Yang, Y. D. Yang, G. F. Zhang, P. Wu
A considerable amount of waste slag from the pyrite roasting process is discharged every year. Recovery of iron from the waste slag is of great interest for comprehensive use of mineral resource, redu
Jan 1, 2011
-
The Change in Operating Philosophy After Converting the Comminution Circuit from a Single Stage SAG Mill to a SAG/Ball Mill Circuit ? The Tarkwa Experience
The comminution circuit at Tarkwa Gold Mine was commissioned as a Single Stage SAG mill operated in closed circuit with hydrocyclones designed to process 4Mtpa. The circuit was later expanded by addin
Jan 1, 2012
-
Magnetic Ion Exchange (MIEX) Resin for the Removal of Chromium(VI), Molybdenium(VI), Vanadium(V) And Arsenic(V) Ions from Aqueous Solutions - A Preliminary Batch Study
By R. Hans
Removal of toxic anions from aqueous solution was studied using a Magnetic Ion Exchange (MIEX) resin which is a polyacrylic, strong base resin. Gravity based settling is made more efficient due to the
Jan 1, 2014
-
Study of the Kinetics of Leaching Gold from a Soft Sulphide Ore at the Sadiola Mine
By T. Mulpeter, G. Deschênes
Sadiola Gold Mine is an open pit operation located in Mali and owned by Anglogold Ashanti Ltd, Iamgold Corporation and the State of Mali. A conventional cyanidation process (cyanidation/CIP) treats 15
Jan 1, 2005
-
Structural Geology of the Osisko Lake Area, Quebec
By H. J. Conolly
The area around Osisko lake, the Horne mine, and the town of Rouyn, in northwestern Quebec, presents a most interesting structural problem. The present discussion is confined to an area around Osisko
Jan 1, 1936
-
Mid-Magnitude-Events: A Quantitative approach for run-out assessment taking fragmentation into account
By K. Thuro, B. Sellmeier, M. Krautblatter
"Recent rockfall events, like the Tramin rockfall at January 21st, 2014, underline the significance of a comprehensive hazard assessment. A common way of estimating the hazard along infrastructure is
Jan 1, 2015
-
Springback in Aerospace Sheet Metal Materials
By J .. A. Nemes, I. Ragai
This paper discusses one of the common problems associated with sheet metal forming processes, which is spring back. The materials presented here, stainless steel 410 and Inconel 718, are commonly use
Jan 1, 2006
-
Synthesis of nano-phase titanium carbide by Mg-thermal reduction process
By J. H. Baek, S. Alexandrovskii, D. W. Lee, B. K. Kim
Nano-phase titanium carbide was synthesized by Mg-thermal reduction process using a novel route of Mg-thermal reduction. The processes are based on I) feeding of TiC14+CxC14 x = 1, 2 ) solution into l
Jan 1, 2004
-
Brazing Characteristics of Warm Formed Automotive Heat Exchanger Components
By K. B. Han, S. Winkler, M. J. Benoit, M. J. Worswick
"Automotive heat exchangers are fabricated by forming multi-layered aluminum (Al) alloy brazing sheets into the desired geometry and subsequently passing the assembly through a furnace for brazing. As
Jan 1, 2018