OFR-184-84 Oil Shale Creep Testing At Elevated Temperatures
    
    - Organization:
 - The National Institute for Occupational Safety and Health (NIOSH)
 - Pages:
 - 161
 - File Size:
 - 22773 KB
 - Publication Date:
 - Jan 1, 1983
 
Abstract
An investigation was made to determine the creep behavior of oil shale at elevated temperatures. During the first phase of the investigation, work done on creep behavior of geologic materials was reviewed and triaxial creep tests on oil shale were planned. Tests at temperatures up to 250°C and axial stress up to 3000 psi were conducted at no confinement and at confining pressures equal to 1/3 and 2/3 of axial stress. Wide variations in the elastic properties as well as creep characteristics are exhibited. Creep deformation is more pronounced at elevated temperature but no definite quantitative remarks can be made regarding effect of grade of oil shale due to wide scatter and limited number of data paints. Primary creep can be described by a power law. Secondary creep seems to be an experimental function of deviatoric stress. Teritary creep was not observed within the test duration (24 hours in most tests).
Citation
APA: (1983) OFR-184-84 Oil Shale Creep Testing At Elevated Temperatures
MLA: OFR-184-84 Oil Shale Creep Testing At Elevated Temperatures. The National Institute for Occupational Safety and Health (NIOSH), 1983.